injection molding processing in PA66 nylon shrinkage rate is how much
PA6 series molding shrinkage
名称 and 描述PA66 shrinkage rate molding shrinkage % 备注
15% glass fiber reinforced PA6 0.5-0.8 PA6G15
20% glass fiber reinforced PA6 0.4-0.6 PA6G20
30% glass fiber reinforced PA6 0.3-0.5 PA6G30
40% glass fiber reinforced PA6 0.1-0.3 PA6G40
50% glass fiber reinforced PA6 0.1-0.3 PA6G50
25% glass fiber reinforced flame retardant PA6 0.2-0.4 Z-PA6G25
30% glass fiber reinforced flame retardant PA6 0.2-0.4 Z-PA6G30
30% glass fiber reinforced flame retardant PA6 0.2-0.4 Z-PA6G30
无卤 flame retardant PA6 0.8-1.2 Z-PA6
30% mineral filled flame retardant PA6 0.5-0.8 Z-PA6M30
30% glass beads filling PA6 0.8-1.2 PA6M30
30% glass fiber (GF) material composite/compounding filling PA6 0.3-0.5 PA6M30
40% glass fiber (GF) material composite/compounding filling PA6 0.2-0.5 PA6M40
30% mineral filled PA6 0.6-0.9 PA6M30
40% mineral filled PA6 0.4-0.7 PA6M40
PA6 generally injection molding grade 1.4-1.8 PA6
PA6 fast speed molding 1.2-1.6 PA6
PA6 generally toughened 1.0-1.5 PA6
PA6 in and other toughened 0.9-1.3 PA6
PA6 ultra- toughened 0.9-1.3 PA6
MoS2 filling wear resistant PA6 1.0-1.4 PA6
PA66 series molding shrinkage
名称 and molding shrinkage % 备注
15% glass fiber reinforced PA66 0.6-0.9 PA66G15
20% glass fiber reinforced PA66 0.5-0.8 PA66G20
25% glass fiber reinforced heat resistant 油PA66 0.4-0.7 PA66G25
30% glass fiber reinforced PA66 0.4-0.7 PA66G30
30% glass fiber reinforced hydrolysis resistant PA66 shrinkage rate 0.3-0.6 PA66G30
40% glass fiber reinforced PA66 0.2-0.5 PA66G40
50% glass fiber reinforced PA66 0.1-0.3 PA66G50
25% glass fiber reinforced flame retardant PA66 0.2-0.4 Z-PA66G25
30% glass fiber reinforced flame retardant PA66 0.2-0.4 Z-PA66G30
30% mineral filled flame retardant PA66 0.2-0.4 PA66M30
无卤 flame retardant PA66 0.8-1.2 Z-PA66
30% mineral filled flame retardant PA66 0.4-0.7 Z-PA66M30
30% glass beads filling PA66 0.8-1.2 PA66M30
30% glass fiber (GF) material composite/compounding filling PA66 0.2-0.5 PA66M30
30% mineral filled PA66 0.6-0.9 PA66M30
40% mineral filled PA66 0.4-0.7 PA66M40
generally injection molding grade PA66 1.5-1.8 PA66
fast speed molding PA66 1.5-1.8 PA66
generally toughened PA66 1.2-1.7 PA66
in and other toughened PA66 1.2-1.6 PA66
ultra- toughened PA66 1.2-1.6 PA66
MoS2 filling wear resistant PA66 shrinkage rate 1.2-1.6 PA66